June 8, 2007 at 4:21 pm
#1209
dave chiles
Participant
The problem is not the butt weld of joints and flanges. The problem, I think, is the longitudinal weld of welded pipe itself. The pipe runs can be many feet long so any honeing or machining along the axial length is not an option. There must be a ASME/ASTM spec for the alowable tolerance of the flash weld produced when making welded seamed pipe.